Skip to content
All materials

Copper alloys

Osprey® GRCop-42

Osprey® GRCop-42 is a high-conductivity, high-strength, dispersion-strengthened copper alloy, designed to withstand service temperatures above 500°C.

Chemical composition, %

Si
≤0.035
Cr
3.1-3.4
Cu
Bal.
Nb
2.7-3.0*
Al
≤0.04
O
≤0.05
Fe
≤0.025

Suitable processes

  • Additive manufacturing